Injection how to deal with the masterbatch
Time:[2012-6-26] Views:9165
Masterbatch caused by a common phenomenon in injection molding production:Color and uneven causes: material cylinder temperature, forming a long cycle and resin compatibility is not good.
Approach: to reduce the material cylinder temperature, good compatibility with the carrier.
The gloss is not good cause: low temperature outside the nozzle, forming a long cycle, in the titanium dioxide masterbatch, Masterbatch pigment dispersion.